Lab recipe
For 1 liter, in the order it is made
Last changed on or before , while the collection was at UMass Amherst. Not yet reviewed at Tufts.
1 Dissolve the components
Phytotech Orchid Replate Medium 35.81 g Phytotechlab P7812 Make up to 1 L with water and adjust the pH to 5.8
3 Add the gelling agent
Gelrite 5 g Plantmedia.com 30634003-44 Autoclave at 121 °C for 15 to 20 minutes
5 Add the vitamin solution, then pour
Gamborg B5 Vitamin Mix, 112 mg/mL (1,000X) 1 mL Plantmedia.com 30630027-1